TABOREX TA 2156 MD contains the cross-linking catalyst and stabilizer package. In addition it carries additives that protect the polymer from degradation caused by metal ions. Together with Silon's Silane grafted TABOREX Compounds this master batch completes a Sioplas System (PE-Xb). Application: TABOREX TA 2156 MD is a catalyst Masterbatch according to the Sioplas System for the production of pipes for sanitary and heating applications. TABOREX TA 2156 MD is specifically designed for the use in heterogeneous pipe systems or in systems using brass fittings for pipe jointing. Information provided by Silon US LLC. |