MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess Solbrol® CP Caprylyl glycol and Phenethyl alcohol
Categories: Other Engineering Material

Material Notes: Solbrol® CP is a preservative-free blend of Caprylyl glycol and Phenethyl alcohol that offers synergistic broad spectrum antimicrobial protection.

Application:

  • Skin care products like face creams, body lotions and others
  • Surfactant based formulations like shower gels
  • Recommend dosage: 0.5% to 1.5%
  • Stable and active over a pH range of 4 to 8
  • Can be processed at temperatures up to 80°C
  • Prolonged heating at elevated temperatures is not recommended

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solubility in Water 0.60 %0.60 %
pH 4.64.60.5% in water
 
Descriptive Properties
AppearancePale yellow liquid; slightly viscous
Color<50Hazen
Content39.75-40.25%Caprylyl glycol
 59.75-60.25%Phenethyl alcohol
Specifications>50%solubility in ethanol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8168 / 208561

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.