MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® L-GF30 BK 9.7506 Nylon 12, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 30% Glass Fiber Filled

Material Notes: VESTAMID® L-GF30 BK 9.7506 is a glass fiber–reinforced heat stabilized Polyamide 12 for injection molding. The material contains about 30% glass fibers, an ageing protective agent and a processing aid for a fast and even form filling. Due to the reinforcement moldings from this compound exhibit a higher strength and good heat resistance. Further advantages of VESTAMID® L-GF30 BK 9.7506 are the characterizing properties of PA12, e.g., low water absorption, good dimensional stability and nearly constant mechanical properties at changing ambient humidity. VESTAMID® L-GF30 BK 9.7506 is supplied as cylindrical granules, ready for processing, in moisture-proof bags. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Automotive and Mobility, Sustainable, Industry and Engineering
Sustainability: Sustainable electricity
Processing: Injection molding
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels
Electrical: Insulating
Conformity: Automotive
Additives: Glass fibers
Special Characteristics: High heat resistant
Color: Black
Additives: Antioxidant agent, Heat stabilizer, Processing aids

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccISO 1183
Water Absorption 0.830 %Sim to ISO 62
Moisture Absorption 0.440 %Sim to ISO 62
Linear Mold Shrinkage, Flow 0.00200 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.00700 cm/cmISO 294-4, 2577
Melt Flow 9.00 g/10 min
@Load 2.16 kg,
Temperature 275 °C
ISO 1133
 11.0 g/10 min
@Load 21.6 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 73.0
@Time 3.00 sec
ISO 7619-1
Tensile Strength at Break 150 MPaISO 527
Tensile Strength 150 MPaISO 527
Tensile Strength, Yield 150 MPaISO 527
Elongation at Break 4.50 %Nominal; ISO 527
Elongation at Yield 4.00 %ISO 527
Tensile Modulus 12000 MPaISO 527
Flexural Strength 240 MPaISO 178
Flexural Modulus 11500 MPaISO 178
Flexural Strain at Break 4.00 %ISO 178
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eU
 90.0 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eU
Charpy Impact, Notched 17.0 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eA
 25.0 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 62631-3-1
Dielectric Constant 3.80
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 4.90
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 31.0 kV/mmAC, S20/P50; Sim. To IEC 60243-1
 33.0 kV/mmAC, S20/S20, t.; IEC 60243-1
Dissipation Factor 0.0320
@Frequency 1.00e+6 Hz
IEC 62631-2-1
 0.0510
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 14.0 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 131 µm/m-°C
@Temperature 25.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 177 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 179 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 172 °CISO 75-1/-2
Vicat Softening Point 175 °C
@Load 5.10 kg
50 K/h; ISO 306
 177 °C
@Load 1.02 kg
50 K/h; ISO 306
Glass Transition Temp, Tg 41.0 °CISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
 HB
@Thickness 3.20 mm
IEC 60695-11-10
 HB
@Thickness 0.800 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 °CInjection Molding; ISO 294
 280 °C
Mold Temperature 60.0 °C
 80.0 °CInjection Molding; ISO 294
Injection Velocity 200 mm/secInjection Molding; ISO 294
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7917 / 325049

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.