MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil LDPE LD 150BW Wire & Cable Low Density Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD 150BW is a LDPE containing suitable for the production of LV and MV crosslinked insulation using the 1-step or 2-step silane technology. Through in-house compounding it can also be used in Medium Voltage peroxide cross-linkable insulation. Sufficient antioxidant and Cu-inhibitor should be added to meet specific ageing requirements.

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • LV Silane cross-linkable insulation – 1 step process
  • MV/HV peroxide cross-linked insulation

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ExxonMobil method
Melt Flow 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50
@Time 15.0 sec
50
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 13.8 MPa2000 psiASTM D638
Tensile Strength, Yield 11.7 MPa1700 psiASTM D638
Elongation at Break 580 %580 %ASTM D638
Elongation at Yield 20 %20 %ASTM D638
Flexural Modulus, 1% Secant 221 MPa32000 psiASTM D790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.00e+15 ohm-cm6.00e+15 ohm-cmASTM D257
Dielectric Constant 2.12.1ASTM D150
Dielectric Strength 51.2 kV/mm1300 kV/inASTM D149
Dissipation Factor 0.000100.00010ASTM D150
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 109 °C<= 228 °FPeak Melting Point; ExxonMobil method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LDPE LD 150AC Low Density Polyethylene Resin
Teknor Apex Telcar® TL-8451 Thermoplastic Elastomer
ExxonMobil LDPE LD 615BA Low Density Polyethylene Resin (European Grade)
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin (European Grade)
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin

PEX99259 / 175495

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.