Sinpolene MBW1391 is a polyethylene-based pure white masterbatch designed specifically for use in tubular film blowing, blow molding and extrusion of polyolefins. With its high pigment loading, it offers high coloring value with excellent quality and performance. The blue undertone of this masterbatch is attributed by specially selected high performance, fine crystal size rutile titanium dioxide. It is delivered as free flowing pellets for processing convenience. Characteristic: - Easy processing