MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
301 Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Type 301 is a high strength grade of steel. Its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent choice for decorative structural applications.

Applications include automobile molding and trim, wheel cover, conveyor belts, kitchen equipment, roof draining systems, hose clamps, springs, truck and trailer bodies, railway and subway cars. By varying the chemical composition within the limits set by the ASTM Specifications and by temper rolling, a broad range of magnetic and mechanical properties can be obtained for a variety of applications.

Information provided by Allegheny Ludlum Corporation, Eagle Brass, and the reference(s).

Key Words: UNS S30100; EN 10088/2(95) 1.4310
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.03 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 217
Tensile Strength, Ultimate 515 MPa
Tensile Strength, Yield 205 MPa
Elongation at Break 40 %
Modulus of Elasticity 212 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000720 ohm-cm
Magnetic Permeability <= 1.02H = 200 Oersted, Annealed
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.6 µm/m-°C
@Temperature 20.0 - 100 °C
 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
 18.6 µm/m-°C
@Temperature 20.0 - 500 °C
 19.5 µm/m-°C
@Temperature 20.0 - 700 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 113 BTU-in/hr-ft²-°F
Melting Point 1399 - 1421 °C
Solidus 1399 °C
Liquidus 1421 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 16 - 18 %
Iron, Fe 70.7 - 78 %As Balance
Manganese, Mn <= 2.0 %
Nickel, Ni 6.0 - 8.0 %
Nitrogen, N <= 0.10 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
304 Stainless Steel
302 Stainless Steel, annealed strip
303 Stainless Steel, annealed
410 Stainless Steel
Overview of materials for T 300 Series Stainless Steel

MQ301 / 12620

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.