MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ITW Devcon® Flexane Polyurethane Putty
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: A tough fast curing rubber urethane compound for sealing, repairing and molding applications. Application: • Lines process equipment to dampen noise • Potting and encapsulating compounds • Repairs and rebuilds conveyor belts • Gouge repair in rubber belting • Gasket sealer • RASH tile sealing.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/cc
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8787
Tensile Strength 23.5 MPa3410 psi
Elongation at Break 200 %200 %
Tear Strength 53.5 kN/m305 pli
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 14.0 kV/mm356 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 48.9 °C120 °FTemperature Resistance - Wet
 82.2 °C180 °FTemperature Resistance - Dry
Shrinkage 0.070 %0.070 %Linear During cure
 
Processing PropertiesMetricEnglishComments
Cure Time >= 600 min>= 10.0 hour
Pot Life 25.0 min25.0 min
 
Descriptive Properties
Chemical/Solvent ResistanceAmmonia: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Cutting Oil: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Gasoline (Unleaded): poor30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric 37%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Isopropyl Alcohol: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Methyl Chloride: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Methyl Ethyl Ketone: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 50%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hypochlorite 5% (bleach): fair30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric 98%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Xylene: fair30 day immersion at 75°F. Sample cured 7 days at RT
ColorBlack
Coverage0.848m²/Kg@ 1mm
Mix Ratio by volume2 to 1
Mix Ratio by weight2.52 to 1
Specific Volume (in.³/lb)23.5
Viscosityputty

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWD9192 / 239702

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.