MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Clariant OMAN698583 Thermoplastic Polyurethane, Halogen Free, Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Aromatic Polyether Based

Data provided by Clariant Masterbatches

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 88ASTM D2240
Tensile Strength, Yield 3100 psiASTM D412
Tensile Stress at Strain 750 psi
@Strain 100 %
ASTM D412
 1300 psi
@Strain 300 %
ASTM D412
Elongation at Break 620 %ASTM D412
Tear Strength 340 pliDie C; ASTM D624
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
@Thickness 3.17 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 360 - 380 °F
Middle Barrel Temperature 370 - 380 °F
Front Barrel Temperature 370 - 380 °F
Melt Temperature 370 - 385 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Miracll E180F Halogen-Free Flame Retardant TPU
Austin Novel Materials Texalan® 598A Polyether-based TPU
Austin Novel Materials Texalan® 698A Polyester and Polyether based TPU
BASF Elastollan® 1154 D KFFC TPUR
3M Scotchcast™ 2131 Flame-Retardant Compound

PCLAR064 / 82189

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.