MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECATRON SX natural Polyphenylene Sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS); Molded

Material Notes:
  • good heat deflection temperature
  • good chemical resistance
  • resistance against high energy radiation
  • high strength
  • high dimensional stability
  • high stiffness
  • high creep resistance
Target Industries:
  • semiconductor technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.36 g/cc
Water Absorption 0.010 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 103.9ISO 2039-1
Hardness, Shore D 85.2ASTM D 2240
Tensile Strength at Break 14200 psiASTM D638
Tensile Strength, Yield 15120 psiASTM D638
Elongation at Break 4.98 %ASTM D638
Modulus of Elasticity 597.8 ksiASTM D638
Flexural Strength 22400 psiASTM D790
Flexural Modulus 596800 psiASTM D790
Compressive Yield Strength 20560 psi
@Strain 10 %
ASTM D695
Compressive Strength 4376 psi
@Strain 1 %
ASTM D695
Compressive Modulus 429400 psiASTM D695
Izod Impact, Notched 0.580 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmDIN IEC 60093
Surface Resistance 1.00e+14 ohmDIN IEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 33.3 µin/in-°F
@Temperature 22.8 - 60.0 °C
DIN EN ISO 11359-1;2
 38.9 µin/in-°F
@Temperature 22.8 - 100 °C
DIN EN ISO 11359-1;2
 66.7 µin/in-°F
@Temperature 100 - 150 °C
DIN EN ISO 11359-1;2
Specific Heat Capacity 0.239 BTU/lb-°FISO 22007-4:2008
Thermal Conductivity 1.74 BTU-in/hr-ft²-°FISO 22007-4:2008
Melting Point 543 °F
Maximum Service Temperature, Air 446 °Flong term
 500 °Fshort term
Glass Transition Temp, Tg 341 °F
Flammability, UL94 HBDIN IEC 60695-11-10
 
Descriptive Properties
Colorbeige opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN8235 / 319163

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.