MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Akrochem PEG 3350 Polyethylene Glycol
Categories: Other Engineering Material

Material Notes: Product Description: PEG 3350 is an effective activator employed when compounding with silica and clay fillers. PEG 3350 overcomes the retarding effect caused by various mineral pigments, improving both cure rate and state of cure. PEG 3350 also functions as a process aid in rubber compounds, which may otherwise be difficult to process. Lubrication and release of EPDM extrusions (including black-loaded compounds) is much improved. The presence of PEG 3350 in EPDM will also reduce accelerator bloom and iridescence due to the polarity added to the polymer. The polarity promotes microwave curing of EPDM. In addition, PEG 3350 can function as a mandrel or mold release for foam and mechanical goods. PEG 3350 is suitable for use in all types of polymers using non-black fillers. Typical dosages range from 1.5 to 3.0 phr. Up to 4 phr is used in EPDM extrusions. PEG has FDA status under 175.105 and 178.3750. Polyethylene glycols used in rubber vary in molecular weight from 2000 to 8000 with the PEG 3350 covering virtually all general applications.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/cc
pH 6.06.05% Aq
Molecular Weight 3350 g/mol3350 g/mol
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.020 %0.020 %
 
Descriptive Properties
Appearancewhite flakes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH421 / 315339

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.