MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Hyperzone HY55430S HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Hyperzone HY55430S is a high density polyethylene resin that exhibits excellent processability and environmental stress crack resistance. Typical applications include bottles for household chemicals, food products, and personal care products. This resin contains synthetic antistat.

Status: Commercial – Active

Availability: Asia-Pacific; Europe; North America

Application: Bottles For Consumer Goods

Market: Rigid Packaging

Processing Method: Extrusion Blow Molding

Attribute: Excellent ESCR (Environmental Stress Cracking Resistance); Excellent Processability

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.954 g/cc0.0345 lb/in³ASTM D1505
ESCR 100% Igepal® 200 hour200 hourCond B; ASTM D1693
Melt Flow 0.340 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.340 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
PENT 12.0 hour
@Pressure 6.00 MPa,
Temperature 50.0 °C
12.0 hour
@Pressure 870 psi,
Temperature 122 °F
FNCT, 2% Arkopal N100; ISO 16770
Hardness, Shore D 68.068.0ASTM D2240
Tensile Strength, Yield 27.6 MPa4000 psiASTM D638
Elongation at Break >= 1000 %>= 1000 %ASTM D638
Elongation at Yield 9.00 %9.00 %ISO 527-1, -2
Tensile Modulus 1.15 GPa167 ksiISO 527-1, -2
Flexural Modulus 1.31 GPa190 ksi1% Secant; ASTM D790
Tensile Impact Strength 294 kJ/m²140 ft-lb/in²ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 66.0 °C151 °FUnannealed; ASTM D648
Vicat Softening Point 75.0 °C167 °FB50; ISO 306
 127 °C261 °FA50; ISO 306
Brittleness Temperature <= -76.0 °C<= -105 °FF50; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9633 / 324568

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.