MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Inno-Comp INNOPOL® CS 1-2120 AP 20% Talc Filled Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: INNOPOL CS 1-2120 AP is a 20 % talc filled compound based on polypropylene homopolymer. This grade is available in natural and custom colored form.

INNOPOL® CS 1-2120 AP is recommended especially for producing products, where high strength, low warpage, long term heat stability and excellent processability are required.

Information provided by INNO-COMP

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 230 °C
nozzle diam 2.095 mm; ISO 1133
Storage Temperature <= 60.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 34.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Yield 5.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2600 MPa1 mm/min; ISO 527-1,-2
Flexural Modulus 2700 MPaISO 178
Charpy Impact Unnotched 20.0 kJ/m²
@Temperature 0.000 °C
ISO 179/1eU
 35.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.60 kJ/m²
@Temperature 0.000 °C
ISO 179/1eA
 2.60 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 125 °CISO 75-1,-2
Vicat Softening Point 96.0 °CB120; ISO 306
 153 °CA120; ISO 306
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 190 - 240 °CInjection
Middle Barrel Temperature 190 - 240 °CInjection
Front Barrel Temperature 190 - 240 °CInjection
Melt Temperature 210 - 250 °CInjection
Mold Temperature 15.0 - 50.0 °C
Moisture Content <= 0.070 %
 
Descriptive Properties
Resin DesignationPP-H TD 20ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Washington Penn Homopolymer Polypropylene 30% Calcium Carbonate Filled
Inno-Comp INNOPOL® CS 1-7120 AP 20% Talc Filled Polypropylene Homopolymer
ExxonMobil Exxtral™ HMU 404 Performance Polyolefin
ExxonMobil Exxtral™ HMU 210 Performance Polyolefin
ExxonMobil Exxtral™ CMW 402 Performance Polyolefin

PINNO901 / 150101

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.