MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kazanorgsintez 108-279 Low Density Polyethylene Composition with Improved Processibility
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Wire/Cable Grade

Material Notes: Production Method: Compositions are produced from low density polyethylene with additives.

Application: Intended for cable core lapping.

Information Provided by Kazanorgsintez

Key Words: LDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 - 0.925 g/cc0.0331 - 0.0334 lb/inĀ³
Environmental Stress Crack Resistance >= 3.0 hour>= 3.0 hour
Melt Flow 1.5 - 2.5 g/10 min1.5 - 2.5 g/10 min
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant <= 2.3
@Frequency 1000 Hz
<= 2.3
@Frequency 1000 Hz
Dielectric Strength >= 40.0 kV/mm>= 1020 kV/inSample of 1 mm thickness, Alternating current
Dissipation Factor <= 0.00030
@Frequency 1000 Hz
<= 0.00030
@Frequency 1000 Hz
 
Descriptive Properties
Amount of impurities [pcs]2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKAZAN168 / 127487

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.