MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Tefzel® HT-2127 Fluoropolymer Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: Because they offer mechanical strength and toughness together with resistance to heat and chemicals, DuPont™ Tefzel® fluoropolymer resins are widely used to make compact wire and cable constructions that provide long, reliable service in demanding environments. In addition, Tefzel® resins offer easy processing, high specific dielectric strength, and a low coefficient of friction.

Tefzel® HT-2127 retains these traditional characteristics of Tefzel® resins while providing some new property advantages. The advantages offered by Tefzel® HT-2127 include greater flexibility, improved retention of tensile properties at elevated temperatures, reduced flammability, and long-term service life at potentially higher temperatures compared to other Tefzel® resins.

Tefzel® HT-2127 will have the same temperature rating (150°C [302°F]) as other Tefzel® resins.

Applications

The relatively low flexural modulus of Tefzel® HT-2127 means that compared with Tefzel® 200, it can be used as a thicker wall insulation on a given conductor for greater durability while retaining the same degree of flexibility. It can also be used in large diameter constructions to reduce stiffness. Wire insulated with Tefzel® HT-2127 could find use in industries where its special performance attributes are needed. In electronic control assemblies, for example, increased flexibility may be an asset during manufacturing.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Key Words: Ethylene Tetrafluoroethylene Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.75 - 1.79 g/ccASTM D792
Melt Flow 7.0 g/10 minASTM D3159
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 38.0 MPaASTM D1708
 3.50 MPa
@Temperature 200 °C
ASTM D1708
Tensile Strength, Yield 6.00 MPa
@Temperature 180 °C
ASTM D1708
Elongation at Break 300 %ASTM D1708
 600 %
@Temperature 180 °C
ASTM D1708
Flexural Modulus 0.645 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 245 - 250 °CASTM D3159
Oxygen Index >= 34 %
 
Descriptive Properties
Folding Endurance, # cycles, .18-.20 mm120000

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Tefzel® 750 Fluoropolymer Resin
Chemours Tefzel® 280 Resin Modified ETFE
Chemours Tefzel® HT-2190 Fluoropolymer Resin
Chemours Tefzel® 210 Resin Modified ETFE
Chemours Tefzel® HT-2129 Fluoropolymer Resin

PDU9294 / 33361

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.