MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total Finaprene® 409 Styrene-Butadiene TPE Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE; Styrene-Butadiene

Material Notes: Styrene-Butadiene Copolymer

Description: Finaprene® 409 is a thermoplastic elastomer type radial styrene-butadiene block copolymer (SBS). Because of its high molecular weight, Finaprene® 409 provides excellent mechanical and elastic properties to the roofing sheet.

Applications: Thanks to its high molecular weight Finaprene® 409 is designed for the roofing industry. Its high styrene content, along with the high molecular weight confer an excellent temperature range at a fairly low viscosity and an easy dispersion to the modified bitumen.

Additional Notes:
Oil Content: 5 phr; Finaprene 1010

Data provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measure 19.5 cSt19.5 cStToluene Solution; Finaprene 1008 Test
 
Chemical PropertiesMetricEnglishComments
Styrene Content 31 %31 %Finaprene 1004 Test
Butadiene Content 69 %69 %Finaprene 1004 Test

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Finaprene® 409 Thermoplastic Elastomer
Versalis Europrene® SOL T 161B Styrene - Butadiene Block Copolymer
Versalis Europrene® SOL T 161C Styrene - Butadiene Block Copolymer
Total Finaprene® 411x Thermoplastic Elastomer
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer, 80 Shore A

PFINAP002 / 38589

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.