MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teijin Panlite® G-3420H Glass Fiber Reinforced Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes: Glass Fiber Reinforced grades-20% glass fiber, low anisotropy grade. Availability: Africa, Middle East, Asia Pacific, Europe, Latin America, North America. Filter / reinforcement: Glass fiber, 20% filler by weight. Features: Creep resistant, High Rigidity, low anisotropy. Uses: Camera Applications, industrial applications. Forms: pellets. Processing Method: Injection Molding.

Information provided by Teijin Chemicals Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Moisture Absorption 0.140 %
@Temperature 23.0 °C,
Time 86400 sec
0.140 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Thickness 4.00 mm
0.0020 - 0.0040 in/in
@Thickness 0.157 in
Teijin method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
@Thickness 4.00 mm
0.0040 - 0.0060 in/in
@Thickness 0.157 in
Teijin method
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 3.0 %3.0 %ISO 527-2/5
Tensile Modulus 5.00 GPa725 ksiISO 527-2/1
Flexural Strength 135 MPa19600 psi2.0 mm/min; ISO 178
Flexural Modulus 5.00 GPa725 ksi2.0 mm/min; ISO 178
Charpy Impact Unnotched 5.80 J/cm²27.6 ft-lb/in²ISO 179
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant  3.4
@Frequency 100 Hz
3.4
@Frequency 100 Hz
IEC 60250
 3.4
@Frequency 1e+6 Hz
3.4
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm889 kV/inshort time test; IEC 60243-1
Dissipation Factor  0.0010
@Frequency 100 Hz
0.0010
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 175 V175 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C22.2 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C33.3 µin/in-°FISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 143 °C289 °Funannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 137 °C279 °Funannealed; ISO 75-2/A
Vicat Softening Point 146 °C295 °FISO 306/B50
UL RTI, Electrical 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL 746
UL RTI, Mechanical with Impact 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL 746
UL RTI, Mechanical without Impact 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL 746
Flammability, UL94  HB
@Thickness 0.430 mm
HB
@Thickness 0.0169 in
 V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
 V-1
@Thickness 3.00 mm
V-1
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teijin Panlite® G-3130PH Glass Fiber Reinforced Polycarbonate
Teijin Panlite® G-3420R Glass Fiber Reinforced Polycarbonate Resin
Teijin Panlite® G-3430R Glass Fiber Reinforced Polycarbonate Resin
E-Glass Fiber, Generic
DuPont™ Kevlar® Aramid Pulp

PTEIH957 / 191637

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.