MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LUPOL GP3156F Flame Retardant PP
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Description: Injection Molding, FR PP, General Purpose, Flame Retardant

Application: Electrical & Electronic, Automotive Parts

CAS: 9003-07-0, 84852-53-9, 14807-96-6 and 1309-64-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.32 g/ccASTM D792
Maximum Moisture Content 0.010Injection Molding
Linear Mold Shrinkage, Flow 0.0090 - 0.013 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 280 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break 20 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Flexural Yield Strength 390 kg(f)/cm²
@Thickness 6.40 mm
10mm/min; ASTM D790
Flexural Modulus 18000 kg(f)/cm²
@Thickness 6.40 mm
10mm/min; ASTM D790
Izod Impact, Notched >= 5.00 kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 120 - 180 secASTM D495
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=0.750 mm
 15 - 30 sec
@Thickness >=1.50 mm
 15 - 30 sec
@Thickness >=2.00 mm
 30 - 60 sec
@Thickness >=3.00 mm
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 0.750 mm
 >= 120 arcs
@Thickness 1.50 mm
 >= 120 arcs
@Thickness 2.00 mm
 >= 120 arcs
@Thickness 3.00 mm
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
@Thickness 3.20 mm
Unannealed; ASTM D648
UL RTI, Electrical 125 °C
@Thickness >=0.750 mm
 125 °C
@Thickness >=1.50 mm
 125 °C
@Thickness >=2.00 mm
 125 °C
@Thickness >=3.00 mm
UL RTI, Mechanical with Impact 120 °C
@Thickness >=0.750 mm
 120 °C
@Thickness >=1.50 mm
 120 °C
@Thickness >=2.00 mm
 120 °C
@Thickness >=3.00 mm
UL RTI, Mechanical without Impact 120 °C
@Thickness >=0.750 mm
 120 °C
@Thickness >=1.50 mm
 120 °C
@Thickness >=2.00 mm
 120 °C
@Thickness >=3.00 mm
Flammability, UL94 V-0
@Thickness >=0.750 mm
 V-0
@Thickness >=1.50 mm
 V-0
@Thickness >=2.00 mm
 V-0
@Thickness >=3.00 mm
 5VB
@Thickness >=2.00 mm
 5VB
@Thickness >=3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 190 - 210 °CInjection Molding
Middle Barrel Temperature 200 - 230 °CInjection Molding
Front Barrel Temperature 200 - 230 °CInjection Molding
Nozzle Temperature 210 - 230 °CInjection Molding
Melt Temperature 200 - 230 °CInjection Molding
Mold Temperature 40.0 - 60.0 °CInjection Molding
Drying Temperature 70.0 - 80.0 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPaInjection Molding
Screw Speed 30 - 60 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance
LG Chemical LUPOL GP1007F Flame Retardant PP
LG Chemical LUPOL GP1000FC Flame Retardant PP
LG Chemical LUMID GP2101BF PA66+GF10%, Halogen Free Flame Retardant
LG Chemical LUPOY GN5001RFD PC/ABS, High Impact

PLAY460 / 148470

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.