MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Carpenter AerMet® 310
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel

Material Notes: AerMet 310 alloy possesses higher hardness and strength than AerMet 100 alloy while maintaining exceptional ductility and toughness. At a 310 ksi (2137 MPa) ultimate tensile strength, AerMet 310 alloy exhibits toughness values equivalent to alloys 20 ksi (138 MPa) lower in strength. The alloy should be considered as a candidate for use in components requiring high strength, high fracture toughness and exceptional resistance to stress corrosion cracking and fatigue.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.288 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 315000 psi
Tensile Strength, Yield 275 ksi
Elongation at Break 14.5 %
Reduction of Area 63 %
Tensile Modulus 2.79e+7 psi
Fatigue Strength 150000 psi
@# of Cycles 1.00e+7
R=-1, Kt=1
Fracture Toughness 71.42 MPa-m½
Charpy Impact 20.0 ft-lbnotched
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.25 %
Chromium, Cr 2.4 %
Cobalt, Co 15 %
Iron, Fe 69.95 %
Molybdenum, Mo 1.4 %
Nickel, Ni 11 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carpenter AerMet® 340
Carpenter AerMet® 100 Aged at 875°F
QuesTek® Innovations Ferrium® C61™ Case-hardened Gear Steel with Ultrahigh-strength Core
Carpenter AerMet® 100 Aged at 900°F
AISI 4140 Steel, oil quenched, 540°C (1000°F) temper, 25 mm (1 in.) round

NCARL4 / 15805

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.