MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC LNP™ THERMOCOMP™ Compound JF004E Polyethersulfone (PESU) (Asia)
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: LNP THERMOCOMP JF004E compound is based on Polyethersulfone (PES) resin containing 20% glass fiber. Added features of this grade include: Easy Molding.

Features: High Stiffness,Easy Molding,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ASTM D792
 1.51 g/cc0.0546 lb/in³ISO 1183
Moisture Absorption 0.400 %0.400 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/in24hrs; ASTM D955
 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/in24hrs; ASTM D955
 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 109 MPa15800 psiISO 527
 114 MPa16500 psiASTM D638
Elongation at Break 2.9 %2.9 %ASTM D638
 2.9 %2.9 %ISO 527
Tensile Modulus 7.35 GPa1070 ksi50 mm/min; ASTM D638
 7.35 GPa1070 ksi1 mm/min; ISO 527
Flexural Strength 183 MPa26500 psiISO 178
 186 MPa27000 psiASTM D790
Flexural Modulus 6.69 GPa970 ksiASTM D790
 7.59 GPa1100 ksiISO 178
Izod Impact Notched 58.0 J42.8 ft-lbASTM D256
Izod Impact, Unnotched 4.27 J/cm8.00 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 73.0 kJ/m²34.7 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 16.0 J11.8 ft-lbpeak; ASTM D3763
Impact Test 4.00 J2.95 ft-lbMultiaxial Impact; ISO 6603
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 205 °C
@Thickness 3.20 mm
401 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 180 °C356 °FUL 746B
UL RTI, Mechanical with Impact 180 °C356 °FUL 746B
UL RTI, Mechanical without Impact 180 °C356 °FUL 746B
Flammability, UL94 V-0
@Thickness 0.810 mm
V-0
@Thickness 0.0319 in
UL 94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81632 / 289579

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.