Description: TECHNYLSTAR polyamide, reinforced with 35% of glass fiber, for injection molding. Characterized by a high fluidity of the melt. Available in: Europe and North America Product Applications: Due to its outstanding flow characteristics, TECHNYLSTAR TM S 216 V35 provides a significant productivity improvement and allows more freedom in mould design and part design versus standard polyamide solutions. This product is available in natural. DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe. |