MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ATI Wah Chang Niobium
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: Niobium is a soft, ductile metal which can be cold worked over 90 percent before annealing becomes necessary. In appearance, the metal is somewhat similar to stainless steel. The density of 8.57 gm/cc is moderate compared to the majority of the high melting point metals, being less than molybdenum at 10.2 gm/cc and only half that of tantalum at 16.6 gm/cc.

Information provided by ATI Wah Chang

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.58 g/cc0.310 lb/in³
a Lattice Constant 3.30 Å3.30 Å
 
Chemical PropertiesMetricEnglishComments
Covalent Radius 1.341.34
Electronegativity 1.61.6Pauling`s
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 60 - 10060 - 100
Modulus of Elasticity 103 GPa14900 ksi
Poissons Ratio 0.380.38
Shear Modulus 37.3 GPa5410 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000150 ohm-cm0.0000150 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.10 µm/m-°C
@Temperature 20.0 °C
3.94 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.320 J/g-°C
@Temperature 1227 °C
0.0765 BTU/lb-°F
@Temperature 2241 °F
Thermal Conductivity  52.22 W/m-K
@Temperature 0.000 °C
362.4 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
 68.92 W/m-K
@Temperature 1600 °C
478.3 BTU-in/hr-ft²-°F
@Temperature 2910 °F
Melting Point 2468 °C4474 °F
Boiling Point 4927 °C8901 °F
Brittleness Temperature -150 °C-238 °F
 
Processing PropertiesMetricEnglishComments
Recrystallization Temperature 900 - 1300 °C1650 - 2370 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Type 316L Stainless Steel, UNS S31603
Aluminum 6061-T6; 6061-T651
Type 316 Cb Austenitic Stainless Steel, UNS S31640 (Composition Spec)
Oxygen-free high conductivity Copper, Soft, UNS C10200
Oxygen-free electronic Copper, UNS C10100

NATIWC01 / 15056

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.