MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lubrizol ESTAGRIP® ST70A Polyether-Type Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: Low durometer soft feel for excellent grip; outstanding adhesion

Uses: Injection Molding - Overmolding

Availability: Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 67 - 73
@Time 5.00 sec
67 - 73
@Time 0.00139 hour
ASTM D2240
Tensile Strength 22.1 MPa3210 psiASTM D412
Tensile Stress at Strain  2.60 MPa
@Strain 100 %
377 psi
@Strain 100 %
ASTM D412
 4.50 MPa
@Strain 300 %
653 psi
@Strain 300 %
ASTM D412
Elongation at Break 850 %850 %ASTM D412
Graves Tear Strength 61.4 kN/m350 plidie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 3333H-18, 1000g; ASTM D3389 B
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -57.0 °C-70.6 °Fby DSC
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 218 °C424 °F
Middle Barrel Temperature 221 °C430 °F
Front Barrel Temperature 227 °C441 °F
Nozzle Temperature 227 °C441 °F
Melt Temperature 227 °C441 °Fpyrometer check of air shot

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polykemi AB POLYelast TPE Z650A Thermoplastic Elastomer, SEBS-based, Co-injection Grade
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
NEU NEUSoft™ 602-60A Ester TPU / SBC blend
Multibase Multi-Flex® TPE A 7020 BLK
Multibase Multi-Flex® A 7005 C TPE Thermoplastic Elastomer

PNOVEON000 / 55265

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.