MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Dyneon™ TFM™ 1700 Modified PTFE Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: Type III, gr. 1 PTFE. Dyneon™ TFM™ 1700 PTFE is a modified polytetrafluoro-ethylene (PTFE) with exceptional chemical and heat resistance properties and a significantly lower melt viscosity giving better particle fusion during sintering and smoother surfaces. Dyneon TFM 1700 PTFE is a non-free-flowing compression molding powder and base material for high-quality Dyneon TFM PTFE compounds.

Data provided by Dyneon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.166 g/ccASTM D4894
Apparent Bulk Density 0.420 g/ccASTM D4894
Particle Size 25 µmASTM D4894
Deformation 2.0 %
@Pressure 15.00 MPa
Permanent; ASTM D621
 4.0 %
@Time 86400 sec,
Pressure 15.00 MPa
ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62Initial; ASTM D2240
 58
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break 33.1 MPaASTM D4894
Elongation at Break 450 %ASTM D4894
Tensile Modulus 0.650 GPaASTM D638
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 3.70 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 57.0 µm/m-°C
@Temperature 30.0 - 100 °C
ASTM E831
 75.0 µm/m-°C
@Temperature 100 - 200 °C
ASTM E831
 92.0 µm/m-°C
@Temperature 200 - 300 °C
ASTM E831
Thermal Conductivity 0.220 W/m-K
@Temperature 100 °C
ASTM D1530
 0.230 W/m-K
@Temperature 250 °C
ASTM D1530
Shrinkage 5.8 %ASTM D4894

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ TFM™ 1700 PTFE
3M Dyneon™ TFM™ 1700 Granular, PTFE
3M Dyneon™ TFM™ 1600 PTFE
3M Dyneon™ TFM™ 2001Z PTFE
3M Dyneon™ TFM™ 1705 PTFE

PDYM00 / 34651

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.