Uses: Nuclear, mineral acids manufacturing and processing facilities, high-temperature gas-phase reactors. Property values are for samples in the metallurgical condition: 1825°F anneal. Information provided by Allvac, An Allegheny Teledyne Company. |
ASTM B 163, B 166, B 167, B 168. |