MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Overview of materials for Epoxy, Electrically Conductive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Master Bond is a leading manufacturer of high performance epoxy adhesives, sealants, coatings, potting/encapsulation compounds and impregnation resins. Our epoxies include one and two part formulations that can be cured at room temperature, with heat or exposure to UV light. Special formulations feature high electrical and/or thermal conductivity and wide service temperature ranges. Visit www.masterbond.com.

Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.940 - 5.30 g/ccAverage value: 2.78 g/cc Grade Count:104
Volatile Organic Compounds (VOC) Content 0.000 - 591 g/lAverage value: 88.7 g/l Grade Count:7
Water Absorption 0.120 - 0.500 %Average value: 0.405 % Grade Count:4
Solubility in Water 0.000 %Average value: 0.000 % Grade Count:4
Particle Size 2.00 - 50.0 µmAverage value: 30.8 µm Grade Count:41
Viscosity 220 - 2.50e+6 cPAverage value: 113000 cP Grade Count:91
Thickness 25.4 - 254 micronsAverage value: 127 microns Grade Count:7
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55.0 - 93.0Average value: 71.0 Grade Count:6
Hardness, Shore D 19.0 - 90.0Average value: 75.7 Grade Count:76
 55.0 - 55.0
@Temperature 75.0 - 75.0 °C
Average value: 55.0 Grade Count:1
Tensile Strength, Ultimate 13.8 - 55.2 MPaAverage value: 35.6 MPa Grade Count:8
Elongation at Break 0.200 - 55.0 %Average value: 35.1 % Grade Count:3
Modulus of Elasticity 0.146 - 7.87 GPaAverage value: 3.73 GPa Grade Count:46
Shear Strength 4.48 - 68.9 MPaAverage value: 15.7 MPa Grade Count:60
 5.15038 - 9.30792 MPa
@Temperature 150 - 250 °C
Average value: 9.39 MPa Grade Count:1
 9.65266 - 11.0316 MPa
@Temperature 65.6 - 116 °C
Average value: 9.39 MPa Grade Count:3
 9.65266 - 11.0316 MPa
@Time 900 - 7200 sec
Average value: 9.39 MPa Grade Count:3
Adhesive Bond Strength 0.621 - 39.3 MPaAverage value: 9.53 MPa Grade Count:52
 1.37895 - 4.13685 MPa
@Temperature 93.3 - 93.3 °C
Average value: 2.76 MPa Grade Count:1
Peel Strength 1.93 - 3.51 kN/mAverage value: 2.98 kN/m Grade Count:3
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000800 - 7.60e+13 ohm-cmAverage value: 5.55e+11 ohm-cm Grade Count:116
 0.000300 - 0.00200 ohm-cm
@Temperature 65.0 - 150 °C
Average value: 0.00364 ohm-cm Grade Count:2
 <= 0.0100 ohm-cm
@Temperature 65.6 - 150 °C
Average value: 0.00364 ohm-cm Grade Count:5
 <= 0.0100 ohm-cm
@Time 900 - 10800 sec
Average value: 0.00364 ohm-cm Grade Count:5
Surface Resistance 0.0100 - 6.00e+6 ohmAverage value: 436000 ohm Grade Count:18
 5.00 - 40.0 ohm
@Temperature 75.0 - 75.0 °C
Average value: 15.0 ohm Grade Count:3
Shielding Effectiveness 40.0 - 120 dBAverage value: 78.8 dB Grade Count:4
Dielectric Strength 2.00 - 19.1 kV/mmAverage value: 10.3 kV/mm Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.50 - 280 µm/m-°CAverage value: 76.8 µm/m-°C Grade Count:72
Thermal Conductivity 0.550 - 29.0 W/m-KAverage value: 2.90 W/m-K Grade Count:78
 10.9 - 23.0 W/m-K
@Temperature 150 - 150 °C
Average value: 17.0 W/m-K Grade Count:1
 10.9 - 23.0 W/m-K
@Time 3600 - 3600 sec
Average value: 17.0 W/m-K Grade Count:1
Maximum Service Temperature, Air 50.0 - 538 °CAverage value: 198 °C Grade Count:113
Minimum Service Temperature, Air -269 - -20.0 °CAverage value: -60.3 °C Grade Count:95
Glass Transition Temp, Tg -5.00 - 155 °CAverage value: 74.3 °C Grade Count:81
Decomposition Temperature 316 - 478 °CAverage value: 398 °C Grade Count:41
Flash Point 7.22 - 150 °CAverage value: 105 °C Grade Count:7
 
Processing PropertiesOriginal ValueComments
Processing Temperature 65.0 - 165 °CAverage value: 106 °C Grade Count:5
Cure Time 1.00 - 10100 minAverage value: 2040 min Grade Count:64
 0.750 - 1440 min
@Temperature 40.0 - 302 °C
Average value: 83.7 min Grade Count:124
Pot Life 10.0 - 130000 minAverage value: 5230 min Grade Count:115
 2880 - 2880 min
@Temperature 5.00 - 5.00 °C
Average value: 2880 min Grade Count:1
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 4.40 - 69.0 %Average value: 22.5 % Grade Count:10
Silver, Ag 40.0 - 85.0 %Average value: 66.3 % Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Adhesive
Overview of materials for Epoxy, Thermally Conductive
Overview of materials for Cyanoacrylate Adhesive
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
Overview of materials for Thermoset Polyurethane, Adhesive

O1725 / 120754

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.