MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Barlog Plastics KEBABLEND M 11/25 PA6 for Plastic Bonded Magnets
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: PA6 functional compound for the production of plastic bonded magnets

Properties: magnetizable

Typical areas of application: Holding magnets, Magnets for sensors, Pumps and motors

Industries: Automotive, Electrical and electronics industry, Household appliances, Mechanical Engineering

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.25 g/ccISO 1183-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 90.0 MPaISO 527-1
Elongation at Break 1.40 %ISO 527-1
Modulus of Elasticity 17.0 GPaISO 527-1
 
Electrical PropertiesOriginal ValueComments
Magnetic Coercive Force, Hc 3142 Oe250 kA/m; DIN EN 60404-5
Magnetic Remanence, Br 2400 Gauss240 mT; DIN EN 60404-5
Magnetic Maximum Energy Product, BH 1.38 MGOe11 kJ/m³; DIN EN 60404-5
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CISO 11357-1/-3
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 - 280 °C
Mold Temperature 80.0 - 100 °C
Drying Temperature 80.0 °C
Dry Time 4.00 - 8.00 hour
Back Pressure 4.00 - 8.00 MPa
 
Descriptive Properties
Magnetic properties11 kJ/m³max. energy product (BH max), DIN EN 60404-5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBARLO424 / 326498

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.