MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK), Very good wear resistance
Categories: Polymer; Thermoplastic; Polyketone

Material Notes: Very good wear resistance, dry and lubricated, high melt flow for injection molding

AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear resistance, the resin also offers the outstanding combination of ultra-performance attributes commonly known for PEEK. These include: chemical resistance, mechanical strength and stiffness, even at elevated temperatures, as well as long-term and high-temperature thermal-oxidative stability. AV-742 SL30 is formulated with the ternary anti-friction/anti-wear additive system comprised of carbon fiber, graphite, and polytetrafluoroethylene (PTFE). It offers wear resistance performance comparable to PEEK grades with this modifier system while being more cost-effective.

This high flowing (low viscosity) grade is designed for use in the injection molding of thin, intricate or complex shapes, or parts in otherwise challenging molding configurations. If the part geometry is such that low viscosity is not a processing necessity, it is recommended that the companion grade AV-722 SL30 be considered first to take advantage of the higher molecular weight of that grade, which results in greater wear resistance as well as better overall mechanical performance in terms of toughness-related properties. The resin can be melt processed using conventional equipment and techniques.

Potential applications for AV-742 SL30 include bushings, bearings, wear strips, wear rings, rollers, and other parts used in sliding friction components. The resin is black in color in its natural state.

Markets/Uses: Automotive / Air Induction / Bushings

Applications: Automotive Applications; Bushings; Thin-walled Parts; Wear Strip

Features: Chemical Resistant; Flame Retardant; Good Dimensional Stability; High Heat Resistance; Wear Resistant

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³ASTM D792
Water Absorption 0.030 %
@Time 86400 sec
0.030 %
@Time 24.0 hour
ASTM D570
Viscosity 270 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
270 cP
@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.18 mm
0.0010 - 0.0030 in/in
@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm
@Thickness 3.18 mm
0.016 - 0.018 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 400 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8787ASTM D785
Tensile Strength 143 MPa20700 psi5.0 mm/min; ASTM D638
Tensile Strength, Yield 156 MPa22600 psiType 1A, 5 mm/min; ISO 527-2
Elongation at Break 1.8 %1.8 %5.0 mm/min; ASTM D638
 1.8 %1.8 %Type 1A, 5 mm/min; ISO 527-2
Tensile Modulus 13.0 GPa1890 ksi5.0 mm/min; ASTM D638
 15.5 GPa2250 ksi1 mm/min, Type 1A; ISO 527-2
Flexural Strength 203 MPa29400 psiISO 178
 211 MPa30600 psiASTM D790
Flexural Modulus 10.4 GPa1510 ksiASTM D790
 13.2 GPa1910 ksiISO 178
Compressive Strength 121 MPa17500 psiASTM D695
Shear Strength 70.0 MPa10200 psiASTM D732
Izod Impact, Notched 0.530 J/cm0.993 ft-lb/inASTM D256
Izod Impact, Unnotched 4.10 J/cm7.68 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 5.80 kJ/m²2.76 ft-lb/in²ISO 180
Izod Impact, Unnotched (ISO) 28.0 kJ/m²13.3 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
5.56 µin/in-°F
@Temperature -58.0 - 122 °F
ASTM E831
Specific Heat Capacity  1.25 J/g-°C
@Temperature 50.0 °C
0.299 BTU/lb-°F
@Temperature 122 °F
ASTM C351
 1.71 J/g-°C
@Temperature 200 °C
0.409 BTU/lb-°F
@Temperature 392 °F
ASTM C351
Thermal Conductivity 0.340 W/m-K2.36 BTU-in/hr-ft²-°FASTM C177
Melting Point 343 °C649 °FPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 276 °C529 °FAnnealed; ASTM D648
Glass Transition Temp, Tg 152 °C306 °FDSC
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 354 °C669 °F
Middle Barrel Temperature 366 °C691 °F
Front Barrel Temperature 371 °C700 °F
Nozzle Temperature 374 °C705 °F
Melt Temperature 366 - 388 °C691 - 730 °FInjection
Mold Temperature 149 - 177 °C300 - 351 °F
Drying Temperature 149 °C
@Time 14400 sec
300 °F
@Time 4.00 hour
 
Descriptive Properties
AdditiveCarbon Fiber + Graphite + PTFE Lubricant
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
Injection RateFast
ProcessingInjection Molding; Machining; Profile Extrusion
Screw Compression Ratio2.0:1.0 to 3.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4157 / 279957

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.