MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

FKuR Kunststoff Bio-Flex® F 2110 Compostable PLA Blend
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any starch or starch derivatives. Bioplastics generally replace conventional materials such as low density polyethylene (LDPE), high density polythene (HDPE) as well as polystyrene (PS) and polypropylene (PP). For packaging applications these materials need to be converted into film which is as thin as possible while maintaining high tensile strength. Depending on the specific application, packaging films have to provide a high barrier against humidity, oxygen and aromas or alternatively provide adequate permeability (“breathability”).

Information Provided by FKuR Kunststoff GmbH

Key Words: Polylactic Acid; biodegradable film
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.770 g/cc0.0278 lb/in³ISO 60
Density 1.27 g/cc0.0459 lb/in³ISO 1183
Water Vapor Transmission 130 g/m²/day
@Thickness 0.0300 mm
8.37 g/100 in²/day
@Thickness 0.00118 in
ISO 15 106-3
Oxygen Transmission Rate 1450 cc/m²/day
@Thickness 0.0300 mm
93.4 cc/100 in²/day
@Thickness 0.00118 in
1 bar; ISO 15 105-2
Nitrogen Transmission 6.99 cc-mm/m²-24hr-atm
@Thickness 0.0300 mm
17.8 cc-mil/100 in²-24hr-atm
@Thickness 0.00118 in
DIN 53380-2
Melt Flow 3.0 - 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 - 5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 49.0 MPa7110 psiMD; ISO 527
Film Tensile Strength at Yield, TD 28.0 MPa4060 psiISO 527
Tensile Strength, Yield 20.0 MPa2900 psiISO 527
Film Elongation at Break, MD 220 %220 %ISO 527
Film Elongation at Break, TD 430 %430 %ISO 527
Elongation at Yield >= 300 %>= 300 %ISO 527
Tensile Modulus 0.340 GPa49.3 ksiFilm, TD; ISO 527
 0.730 GPa106 ksiISO 527
 1.13 GPa164 ksiFilm, MD; ISO 527
Flexural Strength 17.0 MPa2470 psiat 3.5% strain; ISO 178
Flexural Modulus 0.680 GPa98.6 ksiISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1/1eU
Charpy Impact, Notched 8.30 J/cm²
@Temperature 23.0 °C
39.5 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
Elmendorf Tear Strength, MD 0.0441 g/micron1.12 g/milASTM D 1922
Elmendorf Tear Strength, TD 0.120 g/micron3.06 g/milASTM D 1922
 
Thermal PropertiesMetricEnglishComments
Melting Point 145 - 160 °C293 - 320 °FISO 3146-C
Vicat Softening Point 78.0 °C172 °FA; ISO 306
 
Descriptive Properties
Melt Volume Flow (cm3/10 min)3-4ISO 1133; 190°C, 2.16kg
Spencer Impact Test (N/mm)680ASTM D 3420

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
FKuR Kunststoff Bio-Flex® F 6510 Compostable PLA Blend
FKuR Kunststoff Bio-Flex® F 1130 Compostable PLA Blend
FKuR Kunststoff Bio-Flex® F 1110 Compostable PLA Blend
FKuR Kunststoff Bio-Flex® F 2201 CL Compostable PLA Blend
FKuR Kunststoff Bio-Flex® FX 1120 PLA Blend

PFKUR004 / 107042

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.