MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Albis Plastics ABS 01A GP01 Unreinforced  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Amorphous Acrylonitrile Butadiene Styrene Terpolymer (ABS)

Characteristics: General Purpose: Easy Flow, High Impact Strength, High Heat Resistance

Applications: Consumer Appliances, Telecommunication and Automotive Components

Processing: Injection Molding (Melt Temperature: 430-500°F, Mold Temperature: 85-140°F)

Data supplied by Albis Plastics Corporation.

Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Melt Flow 20 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 103ASTM D785
Tensile Strength at Break 43.4 MPaASTM D638
Tensile Strength, Yield 48.3 MPaASTM D638
Elongation at Yield 2.7 %ASTM D638
Modulus of Elasticity 2.36 GPaASTM D638
Flexural Yield Strength 73.8 MPaASTM D790
Flexural Modulus 2.39 GPaASTM D790
Izod Impact, Notched 3.68 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °CAnnealed; ASTM D648
Vicat Softening Point 97.0 °C(rate A, loading 2); ASTM D1525
Flammability, UL94 HB
@Thickness 1.50 mm
Albis Internal Test
 
Processing PropertiesOriginal ValueComments
Melt Temperature 221 - 260 °CInjection
Mold Temperature 29.0 - 60.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PTS Trilac® ABS-HS6500 High Impact ABS Resin
SEKISUI SPI ALLEN® 3800/LXS ABS
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet
Lotte Advanced Materials Starex® SD-0150 ABS, Unreinforced
LG Chemical SG175G ABS, Super Surface Gloss, High Flow

PZA1A07 / 21602

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.