MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay Chemicals Calcium fluoride
Categories: Ceramic; Halide

Material Notes: Calcium fluoride (CaF2) is used in aluminum-metallurgy, brake lining, glass manufacturing, enamel and glazing frits production, dental application, and the production of welding agents.

Calcium fluoride: CAS-No.: 7789-75-5 / EC-No.: 232-188-7

Uses: Metallurgy, Glass industry, Dental application and Brakes

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 1423 °C
Boiling Point 2786 °C
 
Descriptive Properties
AppearanceCrystalline powder
ColorWhite
Composition>95%Calcium fluoride

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech Lutetium Aluminum Garnet:Cerium (LAG:Ce) Scintillator Crystal
Reade Advanced Materials Garnet Powder (Fe3Al2(SiO4)3)
Harris Acoustic Sensors ELL-1203 Aluminum Substituted Narrow Line Width Garnet (3-Series)
Calcium Fluoride, CaF2 (Fluorite)
Mateck Calcium Fluoride (CaF2)

WSOLV011 / 147660

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.