MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Nucrel® 31001 Ethylene-Acrylic Acid Copolymer Resin for Blown and Cast Film
Categories: Polymer; Film; Thermoplastic; Ethylene Acrylic Acid

Material Notes: 9.5 wt% Acrylic Acid.

Nucrel® 31001 is an ethylene-acrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.

Features/Benefits: Excellent adhesion to coextruded nylon for superior structure reliability and barrier integrity. High film strength for excellent structure reliability and product protection. Very good hot tack, sealability through contamination, and heat seal strength for strong, reliable heat seals.

Typical Applications: Meat, poultry, seafood, and cheese packaging. Medical/pharmaceutical packaging. Edible oil, motor oil, and other liquid product pouches. Coextrusions with nylon or in other film structures as a heat seal or tie layer.

Information provided by DuPont Packaging Polymers.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D792
Melt Flow 1.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 490 %50 µm (2 mil) film; ASTM D882
Film Elongation at Break, TD 440 %50 µm (2 mil) film; ASTM D882
Secant Modulus, MD 0.124 GPa50 µm (2 mil) film; ASTM D882
Secant Modulus, TD 0.124 GPa50 µm (2 mil) film; ASTM D882
Impact 31J/mm Spencer Impact; ASTM D3420
Graves Tear Strength 75.3 kN/mTD; ASTM D1004
 81.1 kN/mMD; ASTM D1004
Elmendorf Tear Strength, MD 110 g/mil50 µm (2 mil) film; ASTM D1922
Elmendorf Tear Strength, TD 180 g/mil50 µm (2 mil) film; ASTM D1922
Dart Drop Test 7.90 g
Seal Strength 2500 g/25 mmseal bar 140°C.
Film Tensile Strength at Break, MD 33.0 MPa50 µm (2 mil) film; ASTM D882
Film Tensile Strength at Break, TD 30.0 MPa50 µm (2 mil) film; ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 80.0 °CFreezing Point via DSC/ASTM D3418
 99.0 °CUpon Melting via DSC/ASTM D3418
Vicat Softening Point 79.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 7.0 %ASTM D1003
Gloss 40 %20°; ASTM D2457
Transmission, Visible 30 %%Clarity
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 191 °CTypical Die Temp.
Melt Temperature 190 - 218 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
Dow Nucrel® 30705 Ethylene Acrylic Acid
Dow Nucrel® 30907 Ethylene Acid Copolymer Resin
Dow Nucrel® 3990 Ethylene-Acrylic Acid Copolymer Resin for Extrusion Coating/Laminating
Dow Nucrel® 3990L Ethylene Acrylic Acid

PDUPJL / 33655

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.