MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Unipetrol Light Oil Hydrogenate
Categories: Fluid; Solvent

Material Notes: Oil hydrogenates are a fraction boiling at above approximately 300°C, gained from crude oil through distillation and mild hydrocracking. They are a mixture of light colour hydrocarbons of semi-solid to pasty character under normal conditions, without any notable water or mechanical impurity content. Oil hydrogenates are special intermediates which after distillation treatment and dewaxing by the customer, serve mainly as a basic component for primary lube oil production. Types: Oil hydrogenates are produced in types agreed with customers in compliance with respective sales agreements. Light, medium and heavy hydrogenates are produced with wide viscosity range and viscosity index 85 to 105.

Information provided by Unipetrol RPA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement >= 80Viscosity Index after dewaxing
Viscosity Measure 10 - 20 cSt
@Temperature 50.0 °C
ASTM Color 1.0 - 2.0
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 170 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PUNIP094 / 82954

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.