MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

KLJ Group KANATOL FLAMEGUARD P 100 Phosphate Esters
Categories: Other Engineering Material

Material Notes: Properties: TPPA is the color less solid, usually sold in a flaked form (mp. 48-490C), TPPA is the general purpose monomeric naturally derived triartryl phosphate. It is most widely used among natural Phosphate Ester due to characteristics like weather resistance, fire retardancy, good flexibility and low solubility in water.

Application: TPPA is used as a flame retardant plasticizer for cellulose acetate, photographic safety field which is its major use. Also used as a flame retardant additive in cellulose nitrile, engineering thermoplastic and rigid urethane form. Where compatibility is limited with pure tri phenyl phosphate combination with other plasticizer such as phthalates are used

Chemical Name: TRI PHENYL PHOSPHATE

Molecular Formula: (C 6 H5 O ) PO

CAS Number: 115-86-6

UN. NO.: 3082

EINECS NO.: 204-212-2

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.208 g/cc
@Temperature 60.0 °C
1.208 g/cc
@Temperature 140 °F
ASTM D1045-08
Brookfield Viscosity 17 cP
@Temperature 60.0 °C
17 cP
@Temperature 140 °F
ASTM D445
Molecular Weight 326.29 g/mol326.29 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 47.5 - 49.5 °C118 - 121 °FIS-5762:1970
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %ASTM E203-01
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 9.4 - 9.5 %9.4 - 9.5 %KLJ/QCD/WIN/49
 
Descriptive Properties
Acidity as H3PO4<0.01%ASTM D1613
AppearanceWhite Crystalline Flakes
Color<25Hazen, ASTM D1045-86
Content<0.05%Free Alcohol, KLJ/QCD/WIN/46
 <10 ppmWater Soluble Impurities, BS-1998:1970
 >99%Ester Content, GLC KLJ/QCD/WIN/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKLJ263 / 284284

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.