MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chi Mei Wonderlite® PC-6710 PC Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Transparent, Flame retardant (non-brominated, and non-chlorinated), 3.0 mm V0. Applications: Electrical appliances, outdoor applications (UL 746C f1).

WONDERLITE® is a polycarbonate (PC) resin polymerized using the double hydroxy compounds of bisphenol-A (BPA) and the carbonate compounds of diphenyl carbonate (DPC), produced via our unique transesterification (melting) method. This resin offers glass-like transparency, high heat resistance, ultra high impact resistance, and dimensional stability, making it suitable for a wide range of applications.

Information provided by Chi Mei Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inISO 294-4
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
Melt Volume Rate (ml/10 min.); ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.0 MPa9430 psi50mm/min; ISO 527
Tensile Strength, Yield 60.0 MPa8700 psi50 mm/min; ISO 527
Elongation at Break 120 %120 %50mm/min; ISO 527
Flexural Strength 90.0 MPa13100 psi2mm/min; ISO 178
Flexural Modulus 2.30 GPa334 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  15.0 kJ/m²
@Thickness 3.17 mm,
Temperature -30.0 °C
7.14 ft-lb/in²
@Thickness 0.125 in,
Temperature -22.0 °F
ISO 180/1A
 60.0 kJ/m²
@Thickness 3.17 mm,
Temperature 23.0 °C
28.6 ft-lb/in²
@Thickness 0.125 in,
Temperature 73.4 °F
ISO 180/1A
Charpy Impact, Notched  1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
1/8"; ISO 179
 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
1/8"; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 68.0 µm/m-°C37.8 µin/in-°FISO 11359
Deflection Temperature at 1.8 MPa (264 psi) 125 °C257 °FUnannealed; ISO 75/A
 140 °C284 °FAnnealed; ISO 75/A
Vicat Softening Point  145 °C
@Load 5.00 kg
293 °F
@Load 11.0 lb
50°C/hr; ISO 306
 150 °C
@Load 1.00 kg
302 °F
@Load 2.20 lb
50°C/hr; ISO 306
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHI9949 / 280846

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.