MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ STAT-KON™ Compound EE005E Polyetherimide (PEI) (Americas)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: LNP STAT-KON EE005E compound is based on Polyetherimide (PEI) resin containing 25% carbon fiber. Added features of this grade include: Easy Molding, Electrically Conductive.

Features: High Stiffness,Light-weight Structural,High Heat Resistance,Super Strong (Carbon Fiber Filled),Electrically Conductive,Easy Molding

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
 1.365 g/cc0.04931 lb/in³ASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.160 %0.160 %23°C/50% RH/24 hrs; ASTM D570
 0.230 %0.230 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.00050 - 0.0030 cm/cm0.00050 - 0.0030 in/in24hrs; ASTM D955
 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/in24hrs; ASTM D955
 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 200 MPa29000 psi5 mm/min; ASTM D638
 200 MPa29000 psi5 mm/min; ISO 527
Elongation at Break 1.4 %1.4 %5 mm/min; ASTM D638
 1.4 %1.4 %5 mm/min; ISO 527
Tensile Modulus 18.17 GPa2635 ksi1 mm/min; ISO 527
 18.3 GPa2650 ksi5 mm/min; ASTM D638
Flexural Strength 276 MPa40000 psiISO 178
 277 MPa40200 psiASTM D790
Flexural Modulus 14.32 GPa2077 ksiASTM D790
 15.01 GPa2177 ksiISO 178
Izod Impact Notched 53.0 J39.1 ft-lbASTM D256
Izod Impact, Unnotched 4.48 J/cm8.39 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 29.0 kJ/m²13.8 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 10.0 J7.38 ft-lbpeak; ASTM D3763
Impact Test 7.00 J5.16 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 - 1.00e+6 ohm-cm100 - 1.00e+6 ohm-cmASTM D257
Surface Resistance 100 ohm - 1e+05100 ohm - 1e+05ASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  19.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 19.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
10.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  27.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 27.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 207 °C405 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 207 °C
@Thickness 3.20 mm
405 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 105 °C221 °FUL 746B
UL RTI, Mechanical with Impact 105 °C221 °FUL 746B
UL RTI, Mechanical without Impact 105 °C221 °FUL 746B
Flammability, UL94  V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
UL 94
 5VB
@Thickness >=1.50 mm
5VB
@Thickness >=0.0591 in
UL 94
 5VA
@Thickness >=3.00 mm
5VA
@Thickness >=0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 390 - 400 °C734 - 752 °F
Zone 2 370 - 390 °C698 - 734 °F
Zone 3 380 - 400 °C716 - 752 °F
Melt Temperature 360 - 400 °C680 - 752 °FInjection Molding
Mold Temperature 140 - 180 °C284 - 356 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
 
Descriptive Properties
Screw speed (Circumferential speed)0.2-0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81278 / 289225

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.