Product Description: Formolene® FC2304C is a low density polyethylene offering good balance of optical properties and high stiffness. Formolene® FC2304C is formulated with slip and antiblock for use in applications offering excellent extrusion processing and good balance of film stiffness and optical properties. Availability: North America Features: Good Optical Properties; High Stiffness; Low Density Uses: Blending; Film; Packaging; Shrink Wrap Processing Method: Coextrusion; Extrusion; Film Extrusion Information provided by Formosa Plastic Corporation |