MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LNP™ STAT-KON™ Compound DE0029E Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DE0029E compound is based on Polycarbonate (PC) resin containing 10% carbon fiber. Added features of this grade include: Flame Retardant, Electrically Conductive, Easy Molding.

Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Flame Retardant,Electrically Conductive,Easy Molding

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³ASTM D792
 1.26 g/cc0.0455 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.160 %0.160 %23°C/50% RH/24 hrs; ASTM D570
 0.200 %0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.00060 - 0.0032 cm/cm0.00060 - 0.0032 in/in24hrs; ISO 294
 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/in24hrs; ASTM D955
 0.0029 - 0.0043 cm/cm0.0029 - 0.0043 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 110 MPa16000 psiASTM D638
 117 MPa17000 psiISO 527
Elongation at Break 2.4 %2.4 %ISO 527
 2.5 %2.5 %ASTM D638
Tensile Modulus 7.80 GPa1130 ksi1 mm/min; ISO 527
 8.27 GPa1200 ksi50 mm/min; ASTM D638
Flexural Strength 179 MPa26000 psiASTM D790
 183 MPa26500 psiISO 178
Flexural Modulus 7.58 GPa1100 ksiASTM D790
 8.65 GPa1250 ksiISO 178
Izod Impact Notched 61.0 J45.0 ft-lbASTM D256
Izod Impact, Unnotched 4.53 J/cm8.49 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²14.3 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 17.0 J12.5 ft-lbpeak; ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 10 - 1.00e+6 ohm10 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  23.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
13.1 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 23.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
13.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  34.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
19.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 34.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
19.2 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 144 °C
@Thickness 3.20 mm
291 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 139 °C282 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 141 °C
@Thickness 3.20 mm
286 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94  V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
UL 94
 5VA
@Thickness >=3.00 mm
5VA
@Thickness >=0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 305 - 325 °C581 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81203 / 289150

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.