MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Celanese Celanex® 6400 Polyester (PBT), 40% Glass/Mineral
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass + Mineral Filled

Material Notes: Warp resistant, good surface smoothness

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccASTM D792
Water Absorption 0.040 %ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 86ISO 2039-2
Tensile Strength, Ultimate 107 MPaISO 527
Elongation at Break 2.0 %ASTM D638
Flexural Strength 170 MPaISO 178
Flexural Modulus 11.0 GPaISO 178
Izod Impact, Notched (ISO) 0.410 J/cm²ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.9
@Frequency 100 Hz
Dielectric Strength 22.0 kV/mm
@Thickness 3.17 mm
50% R.H.; ASTM D149
Dissipation Factor 0.017
@Frequency 100 Hz
Comparative Tracking Index 310 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 200 °CISO 75
Flammability, UL94 HB
@Thickness 0.800 mm
UL94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Phenolic, Novolac, Cellulose Filled
Overview of materials for AISI 4000 Series Steel
LG Chemical Phenol
LG Chemical Lupox® LW-5402 Low Warpage PBT, 40% Glass Filled, High Impact
Huntsman Araldite EPN 1138 Epoxy Phenol Novolac

PHCT32 / 45672

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.