MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Carmel Olefins Capilene® HT 75 A Polypropylene Impact Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Description: CAPILENE® HT 75 A is a nucleated and antistatic high flow impact copolymer for injection molding. It is characterized by improved stiffness, medium impact resistance and good organoleptic properties. CAPILENE® HT 75 A has been formulated to allow short cycle time.

Applications: CAPILENE® HT 75 A has been especially developed for injection molding of pails and containers. This grade is also used for the injection molding of furniture, toys, housewares and technical items.

Information provided by Carmel Olefins.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 25.0 MPa50 mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ASTM D638
Flexural Modulus 1450 MPaASTM D790
Izod Impact, Notched 50.0 J/m
@Temperature -20.0 °C
ASTM D256
 70.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °CASTM D648
Vicat Softening Point 147 °C
@Load 1.02 kg
ASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carmel Olefins Capilene® TG 50 Polypropylene Impact Copolymer
Carmel Olefins Capilene® W 77 AV Polypropylene Homopolymer
Carmel Olefins Capilene® TR 50 Polypropylene Impact Copolymer
Carmel Olefins Capilene® TU 75 AV Polypropylene Impact Copolymer
ExxonMobil PP8013L1 Polypropylene Impact Copolymer

PCARM983 / 131158

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.