MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Mobil Velocite 8
Categories: Fluid; Lubricant

Material Notes: The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydraulic, circulation systems and air line oilers where the appropriate viscosity grade is selected. They are formulated from select high-quality, low viscosity base oils and additives that impart good resistance to oxidation and protection from rust and corrosion. They possess very good resistance to foaming and separate readily from water.

High speed spindle bearings in machine tools and equipment where high speeds and fine clearances are involved; Precision grinders, lathes, jig borers and tracer mechanisms; Velocite Oil No 3 is recommended for "zero clearance" type spindle bearings which operate with extremely close clearances; For sleeve type spindle bearings having greater clearances, the choice of viscosity depends on the relation between clearance and spindle speed; Low pressure hydraulic systems where appropriate viscosity is selected; Air line oilers (Mobil Velocite Oil No. 10); For some sensitive instruments such as telescopes, laboratory equipment, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.854 g/cc
@Temperature 15.0 °C
0.0309 lb/in³
@Temperature 59.0 °F
ASTM D4052
Kinematic Viscosity at 40°C (104°F) 15 cSt15 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 3.28 cSt3.28 cStASTM D445
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.0600.060mgKOH/g; ASTM D974
 
Thermal PropertiesMetricEnglishComments
Pour Point -9.00 °C15.8 °FASTM D97
Flash Point 194 °C381 °FASTM D92
 
Descriptive Properties
Copper Strip Corrosion1A3 hrs @ 100°C
Rust Prevention, Distilled WaterpassASTM D665A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil 624 Mobil SHC 600 Series

WEXXON264 / 75689

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.