MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Henkel Loctite® ECCOBOND FP4654 Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Appearance: Black

Cure: Heat Cure

Product Benefits:

  • High purity
  • Low stress
  • Self-leveling
  • Excellent chemical resistance
  • Jettable
  • Excellent thermal stability
Components: One-component

Application: Encapsulation, Damming or Filler

Typical Application: Cavity fill or dam and fill

LOCTITE ECCOBOND FP4654 encapsulant is designed for larger cavity-fill or dam-and-fill applications.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.85 g/cc1.85 g/cc
Filler Content 80 %80 %
Brookfield Viscosity 32000 cP32000 cPSpindle 52, speed 20 rpm
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 16.9 GPa2450 ksiCured, By DMA
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.0 µm/m-°C
@Temperature <=55.0 °C
7.22 µin/in-°F
@Temperature <=131 °F
Cured, Below Tg
 53.0 µm/m-°C
@Temperature 190 - 220 °C
29.4 µin/in-°F
@Temperature 374 - 428 °F
Cured, Above Tg
Glass Transition Temp, Tg 146 °C295 °FCured
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min
@Temperature 125 °C
0.500 hour
@Temperature 257 °F
Plus 90 minutes @ 165°C
Pot Life >= 4320 min>= 4320 mintime to double viscosity
Gel Time 11.0 min
@Temperature 121 °C
11.0 min
@Temperature 250 °F
Shelf Life 9.00 Month
@Temperature -40.0 °C
9.00 Month
@Temperature -40.0 °F
 
Descriptive Properties
Extractable Ionic Content (ppm)10Cured, Sodium (Na+)
 5Cured, Chloride (Cl-)
 5Cured, Potassium (K+)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOCT5085 / 255296

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.