MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Avient Maxxam™ FR PE 161 HDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V-0, and 5VA performance ratings. In addition, many compounds in the Maxxam FR portfolio offer elevated Relative Thermal Index (RTI) ratings.

*HARDNESS DATA IS BASED ON SINGLE LOT DATA.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.998 g/cc0.998 g/ccASTM D792
Melt Flow 0.91 - 2.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.91 - 2.7 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6666ASTM D2240
 65
@Time 10.0 sec
65
@Time 0.00278 hour
ASTM D2240
Tensile Strength, Yield 20.7 MPa3000 psiType I, 51 mm/min; ASTM D638
Elongation at Break 500 %500 %Type I, 51 mm/min; ASTM D638
Gardner Impact 21.5 J
@Thickness 3.18 mm,
Temperature 23.0 °C
15.9 ft-lb
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °C
@Thickness 3.18 mm
153 °F
@Thickness 0.125 in
Annealed; ASTM D648
Flammability, UL94 V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
NC; UL 94
Oxygen Index 27 %
@Thickness 3.18 mm
27 %
@Thickness 0.125 in
ASTM D2863
 
Descriptive Properties
FeaturesFlame Retardant
FormsPellets
Generic NamePolyethylene, High Density (HDPE)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Maxxam® FR PE JR 165 High Density Polyethylene (HDPE)
Ovation Polymers Nima™ HL 18400 HDPE
Avient Maxxam™ FR PE 161-1A Polyethylene, High Density (HDPE)
Multibase Multi-Flam™ 0103 HDPE Polyethylene
Multibase Multi-Flam™ 0103 HDPE NH Polyethylene

PH1PN9123 / 102959

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.