MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Sandvik 19.9.LR Covered electrodes
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 19.9.LR is a covered chromium nickel electrode with rutile-basic coating for welding of steels of ASTM 304 types as well as overlays giving 308 type composition. The electrode has excellent arc stability and fast burn off rate with minimal stub loss. It is also characterized by improved moisture resistance, self peeling slag, easy post weld finishing. Sandvik 19.9.LR gives smooth uniform beads and works in any standard weld position.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 200200
Tensile Strength, Ultimate 600 MPa87000 psi
Tensile Strength, Yield 440 MPa
@Strain 0.2 %
63800 psi
@Strain 0.2 %
Elongation at Break 40 %40 %
Charpy Impact  60.0 J
@Temperature -20.0 °C
44.3 ft-lb
@Temperature -4.00 °F
 75.0 J
@Temperature 20.0 °C
55.3 ft-lb
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.025 %0.025 %
Chromium, Cr 19 %19 %
Manganese, Mn 0.75 %0.75 %
Nickel, Ni 9.5 %9.5 %
Silicon, Si 0.95 %0.95 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSANDV5097 / 199661

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.