MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Desmopan® 3660DU Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Extrusion- and injection molding grade; transparent up to 6 mm wall thickness; hydrolysis-stabilised; with special UV stabilizers; with release agent; good wear resistance; Application; Sports shoe soles; Hoses, non-reinforced; Profiles

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 98ISO 868
Hardness, Shore D 60ISO 868
Tensile Strength, Ultimate 53.7 MPa200 mm/min; DIN 53504
Tensile Stress at Strain 12.1 MPa
@Strain 10 %
200 mm/min; DIN 53504
 22.1 MPa
@Strain 50 %
200 mm/min; DIN 53504
 28.4 MPa
@Strain 100 %
200 mm/min; DIN 53504
 37.8 MPa
@Strain 300 %
200 mm/min; DIN 53504
Elongation at Break 318 %200 mm/min; DIN 53504
Tensile Modulus 0.129 GPa
@Temperature 60.0 °C
storage; ISO 6721-1,-4
 0.444 GPa
@Temperature 20.0 °C
storage; ISO 6721-1,-4
 2.61 GPa
@Temperature -20.0 °C
storage; ISO 6721-1,-4
Rebound 31 %Resilience; ISO 4662
Tear Strength 170 kN/m500 mm/min; ISO 34-1
Abrasion 23mm³, Method A; ISO 4649
Compression Set 24 %
@Temperature 23.0 °C
72 hr; ISO 815
 45 %
@Temperature 70.0 °C
24 hr; ISO 815
 35 %
@Temperature 70.0 °C,
Time 86400 sec
Method C; ISO 815-1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 210 °CExtrusion
 215 - 235 °CInjection
Mold Temperature 20.0 - 40.0 °CInjection
Drying Temperature 110 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmopan® 3491A Polyurethane
Covestro Desmopan® 3055D Polyurethane
Covestro Desmopan® 3072D Polyurethane
Covestro Desmopan® 955 U Polyurethane
Covestro Desmopan® 1350D Polyurethane

PB09793 / 92633

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.