Data provided by the manufacturer, Exxon Chemical. A high vinyl acetate copolymer specialty film resin providing outstanding heat sealability along with excellent strength, properties and clarity. Applications: Heat seal layer in blown and cast coextended films; Pallet stretch wrap. |
Ethylene Vinyl Acetate; Exxon Chemical Company |