MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Aquathene FR420000 W&C Polyolefin Compound
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Aquathene FR420000 is a colorable flame retardant catalyst masterbatch selected by customers for use in moisture cure applications. FR420000 also contains antioxidants, metal deactivator and stabilizers for sunlight resistance. When FR420000 is melt blended with Aquathene AQ120000 in a 52% / 48% ratio, respectively, and crosslinked after exposure to moisture, this formulation is typically used in low voltage power and control cable applications where UL44 and CSA 22.2 (No. 38 and No. 52) specify VW-1 and FT-4 flame rating with 90°C service in wet locations.

Availability: North America

Application: Wire & Cable

Market: Wire & Cable

Processing Method: Wire & Cable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.01 g/cc0.0726 lb/in³ASTM D1505
Melt Flow 2.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.80 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9044 / 323972

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.