MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Aptek 2201-A/B Fast set urethane adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: APTEK 2201-A/B is a two component, dark gray, urethane adhesive system displaying excellent adhesion to various plastic, wood, ceramic, and metal substrates. APTEK 2201-A/B is capable of achieving full cure at room temperature or can be accelerated with moderate heat.

Fast-setting-ideal for field repair, sealing, and patching applications, very good resistance to heat and moisture for outdoor use. Remains flexible over time/aging. Easy to use 1:1 mix ratio. Thixotropic-will not sag on vertical surfaces. Mixes to a third color to ensure a uniform mix. For convenient handling, pre-packaged in tube or dual cartridge kits.

APTEK 2201A is a black, mineral filled polyol resin. APTEK 2201B is a white organic isocyanate.

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccB Component; ASTM D1475
 1.23 g/ccA Component; ASTM D1475
Viscosity 30000 cPA Component; ASTM D1824
 45000 cPB Component; ASTM D1824
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80Cured property; ASTM D2240
Tensile Strength, Ultimate 2200 psiCured property; ASTM D638
Elongation at Break 200 %Cured property; ASTM D638
Adhesive Bond Strength 2000 psiAl-to-Al Lap Shear; Cured property; ASTM D1002; 50 grit, sanded/solvent wiped
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 125 °CA Component; ASTM D92
 >= 125 °CB Component; ASTM D92
 
Processing PropertiesOriginal ValueComments
Processing Temperature 65.0 °CCure 2 hrs; with RT gel

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aptek DIS-A-PASTE 2000-A/B Thermally conductive urethane adhesive
Overview of materials for Thermoset Polyurethane, Adhesive
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive
Abatron AboThane 8003-3 Polyurethane Coating
Aptek 3101 B/C/B Thermally conductive urethane film adhesive

PAPTEK05 / 24167

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.