MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Orion Performance Compounds i-OnComp™ PC GF20 Polycarbonate, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes: 14-102-000-000

Main Features:

  • Natural color
  • Good stiffness
  • High toughness
  • Low mold shrinkage
  • Electrically insulating
Target Industries:
  • Electronics
  • Appliances
  • Automotive

Information provided by Orion Performance Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.36 g/cc1.36 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 105 MPa15200 psiASTM D638
Tensile Strength, Yield 110 MPa16000 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
Tensile Modulus 6.48 GPa940 ksiASTM D638
Flexural Strength 137 MPa19800 psiASTM D790
Flexural Modulus 6.27 GPa910 ksiASTM D790
Izod Impact, Notched 1.17 J/cm2.20 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+12 ohm>= 1.00e+12 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 148 °C298 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 144 °C292 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 299 - 327 °C570 - 620 °F
Zone 1 293 - 310 °C560 - 590 °F
Zone 2 304 - 327 °C580 - 620 °F
Zone 3 304 - 338 °C580 - 640 °F
Melt Temperature 304 - 338 °C580 - 640 °F
Mold Temperature 65.6 - 93.3 °C150 - 200 °F
Drying Temperature 104 °C220 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hour
Moisture Content <= 0.030 %<= 0.030 %
Back Pressure 0.345 - 1.38 MPa50.0 - 200 psi
Screw Speed 30 - 70 rpm30 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PORI9987 / 318020

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.