MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Proto3000 – 3D Engineering Solutions

Taiwan PU APU-32-80B Polyurethane Powder
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Key features:
  • TPU polyester base
  • Glue-line Temperature: 100-120?
  • Diameter: 0-0.1mm, 0.1-0.2mm, 0.2-0.4mm
  • Washing resistance
  • Dry clean resistance
Application: Polyurethane powder can use for digital transfer printing, leather, Neoprene, Lycra textiles & membrane

Features: Washing and dry cleaning resistance

Processing Method: Paste Dot, Powder Dot , Scatter Coating, Laminating Coating

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 10000 cP
@Temperature 160 °C
10000 cP
@Temperature 320 °F
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 150 °C
9.0 g/10 min
@Load 4.76 lb,
Temperature 302 °F
10 min
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595
 
Descriptive Properties
Temperature100-120°CGlue-line
 50°CThermal Stability

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTAIWPU127 / 305857

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.