MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Schott MEMpax® Borosilicate Glass
Categories: Ceramic; Glass

Material Notes: Borosilicate glass manufactured with fire-polished surfaces. It has similar chemical and physical characteristics as the well-known product SCHOTT BOROFLOAT® 33. MEMpax® is available in much lower thicknesses and offers a thin wafer that no longer needs to be ground and polished, thanks to its excellent surface quality. MEMpax® can be used anywhere that extremely thin borosilicate glasses are needed. The coefficient of linear thermal expansion of MEMpax® corresponds with that of silicon, therefore this glass is perfectly suited for use in anodic bonding. Its low autofluorescence, combined with its excellent surface quality, flatness and homogeneity, opens up numerous application possibilities for SCHOTT MEMpax® in MEMS and Biotechnology. Thanks to its low alkali content, MEMpax® acts as a high-quality insulator. For this reason, MEMpax® is an extremely appropriate material for applications that require nonconductive characteristics at high temperatures (up to 450 °C).

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.20 g/cc0.0795 lb/in³Annealed at 40°C/h
Thickness 100 - 700 microns3.94 - 27.6 mil
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.64.6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.25 µm/m-°C
@Temperature 20.0 - 300 °C
1.81 µin/in-°F
@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 525 °C977 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4711.471
Transmission, Visible 97.7 %97.7 %D65

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Corning Pyrex® 7740 Borosilicate Glass Sheet
Schott BOROFLOAT® Borosilicate Float Glass
Borosilicate Glass, Low Expansion
Borosilicate Glass
Mateck Fused Silica IR Grade (SiO2)

CSGT9942 / 183195

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.